X2CrNiMoCuN25-6-3 | 1.4507 Material Datasheet
Unlock Exclusive Materials Data
Gain access to a wealth of materials data by joining our Materials Portal.
Register for Free or Upgrade for Full AccessMaterial Description
Material Number | Material Number (single) | Standard | Range of Application | Standard Status | Country | Predecessor | Successor | Remark |
---|---|---|---|---|---|---|---|---|
1.4507 (DIN EN 10216-5 : 2014-03) | 1.4507 | DIN EN 10216-5 : 2014-03 | DIN EN 10216-5 : 2014-03 replaced by DIN EN 10216-5 : 2021-06 | Replaced | Germany | X2CrNiMoCuN25-6-3 | X2CrNiMoCuN25-6-3 | Seamless stainless steel tube for pressure purposes. |
Chemical Composition
C [%] | Cr [%] | Cu [%] | Mn [%] | Mo [%] | N [%] | Ni [%] | P [%] | S [%] | Si [%] | Source |
---|---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Mechanical Properties
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Specimen Direction | Tensile Strength [MPa] | Yield Strength (0.2% offset) [MPa] | Elongation A [%] | Source |
---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
Physical Properties
Temperature [°C] | Density [g/cm³] | Young's Modulus [GPa] | Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] | Thermal Conductivity [W/(m*K)] | Specific Electrical Resistance [µΩm] | Mean Specific Heat Capacity [kJ/(kg*K)] | Magnetizeability | Source |
---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
Young's Modulus [GPa] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowMean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowToughness Data (Impact)
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Specimen Shape | Specimen Direction | Notch Impact Energy [J] | Source |
---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur |
Heat Treatment
Heat Treatment | Temperature [°C] | Medium | Source |
---|---|---|---|
blur | blur | blur | blur |
Cross Reference
Material Name | Country | Standard | Source |
---|---|---|---|
022Cr24Ni7Mo4CuN | China | GB/T 21833 | Stahlschlüssel 2016, Verlag Stahlschlüssel Wegst GmbH, Marbach |
S25203 | China | GB/T 21833 | Stahlschlüssel 2016, Verlag Stahlschlüssel Wegst GmbH, Marbach |
X2CrNiMoCuN25-6-3 | Europe | EN 10216-5 | |
S32550 | USA | UNS | Metals & Alloys in the Unified Numbering System, SAE/ASTM, 11th Edition, 2008 |
Producer/Supplier/Trade names
Tradename | Supplier |
---|---|
Alloy 255 | Enpar Sonderwerkstoffe GmbH, Gummersbach |
AMINOX 255 | Gourd & Co. Valve, Tube & Alloy Supplies & Services, Schwalbach/Ts. |
FERRINOX 255 | Gourd & Co. Valve, Tube & Alloy Supplies & Services, Schwalbach/Ts. |
DMV 25.7 Cu | Salzgitter Mannesmann Stainless Tubes GmbH, Mülheim an der Ruhr |
Material Compliance
REACh | RoHS |
---|---|
blur | blur |
X2CrNiMoCuN25-6-3 (1.4507; DIN EN 10216-5 : 2014-03)
Linear-elastic
Temperature [°C] | Young's modulus [GPa] | Poisson's ratio |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
Alternating stress
Temperature [°C] | Stress ratio | Alternating stress [MPa] | Cycles |
---|---|---|---|
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Electrical resistivity
Temperature [°C] | Specific electrical resistance [µΩm] |
---|---|
blur | blur |
Coefficient thermal expansion
Related Temperature [°C] | Temperature [°C] | Coefficient thermal expansion [10^-6*K^-1] |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
Specific heat
Temperature [°C] | Specific heat [kJ/(kg*K)] |
---|---|
blur | blur |
Density
Temperature [°C] | Density [g/cm³] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Thermal conductivity
Temperature [°C] | Thermal conductivity [W/(m*K)] |
---|---|
blur | blur |
Classification
WIAM Material | Source description |
---|---|
blur | blur |
Designation
Designation | Material number | Source |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
X2CrNiMoCuN25-6-3 (solution annealed (+AT); tube; 0.000-30.000mm)
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |