EN-GJS-400-18C | 5.3125 Material Datasheet - Properties - Materials Portal

EN-GJS-400-18C | 5.3125 Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access

Material Description

Material NumberMaterial Number (single)StandardRange of ApplicationStandard StatusCountryRemark
5.3125 (DIN EN 16482 : 2024-09)5.3125DIN EN 16482 : 2024-09Supersedes DIN EN 16482 : 2014-09ValidGermanyBars made of spheroidal cast iron (ferritic structure), which have been produced by the continuous casting process.

Chemical Composition

SourceRemark
blurblur

Mechanical Properties

Semi-finished ProductCasting MethodConditionNominal Size [mm]Temperature [°C]Tensile Strength [MPa]Yield Strength (0.02% offset) [MPa]Elongation A [%]Shear Strength [MPa]Torsion Strength [MPa]Hardness HB | HBWSourceRemark
blurblurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblurblur

Physical Properties

Temperature [°C]Density [g/cm³]Young's Modulus [GPa]Bulk Modulus [GPa]Poisson's RatioMean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1]Thermal Conductivity [W/(m*K)]Specific Electrical Resistance [µΩm]Mean Specific Heat Capacity [kJ/(kg*K)]SourceRemark
blurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblur

Young's Modulus [GPa] vs Temperature [°C]

Exclusive Insight Locked!

This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.

Unlock Now

Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]

Exclusive Insight Locked!

This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.

Unlock Now

Magnetic Properties

Temperature [°C]Max. Permeability [µH/m]Hysteresis losses at B=1T [J/m³]SourceRemark
blurblurblurblurblur

Cross Reference

Material NameCountryStandardSource
EN-GJS-400-18CEuropeEN 16482 
Grade 60-40-18USAASTM A536EN 16482 : 2024-07

Producer/Supplier/Trade names

TradenameSupplier
EN-GJS-400-18CACO Guss GmbH, Kaiserslautern
EN-GJS-400-18CContifonte SAS, Saverne
EN-GJS-400-18CGontermann-Peipers GmbH, Siegen
EN-GJS-400-18CHAVO Strangguss GmbH, Kaiserslautern
EN-GJS-400-18CMK Strangguss GmbH, Plettenberg

Fracture Toughness

Casting MethodNominal Size [mm]Temperature [°C]SourceRemark
blurblurblurblurblurblur

EN-GJS-400-18C (5.3125; DIN EN 16482 : 2024-09)

Linear-elastic

Temperature [°C]Young's modulus [GPa]Bulk modulus [GPa]Poisson's ratio
blurblurblurblur
blurblurblurblur
blurblurblurblur

Alternating stress

Temperature [°C]Stress ratioAlternating stress [MPa]Cycles
blurblurblurblur
blurblurblurblur
blurblurblurblur

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Coefficient thermal expansion

Related Temperature [°C]Temperature [°C]Coefficient thermal expansion [10^-6*K^-1]
blurblurblur

Specific heat

Temperature [°C]Specific heat [kJ/(kg*K)]
blurblur
blurblur

Density

Temperature [°C]Density [g/cm³]
blurblur

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur
blurblur

Thermal conductivity

Temperature [°C]Thermal conductivity [W/(m*K)]
blurblur

Classification

WIAM MaterialSource description
blurblur

Designation

DesignationMaterial numberSource
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur


EN-GJS-400-18C (cast condition; casting; 20.000-60.000mm)

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

TreatmentSemi-finished productDimension [mm]Source description
blurblurblurblur


EN-GJS-400-18C (cast condition; casting; 60.000-120.000mm)

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

TreatmentSemi-finished productDimension [mm]Source description
blurblurblurblur


EN-GJS-400-18C (cast condition; casting; 120.000-400.000mm)

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

TreatmentSemi-finished productDimension [mm]Source description
blurblurblurblur


EN-GJS-400-18C (casting; 160.000mm)

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur
blurblur

Classification

Semi-finished productDimension [mm]Source description
blurblurblur