EN AC-Al Si10MnMg | EN AC-43500 Material Datasheet
Unlock Exclusive Materials Data
Gain access to a wealth of materials data by joining our Materials Portal.
Register for Free or Upgrade for Full AccessMaterial Description
Material Number | Material Number (single) | Standard | Range of Application | Standard Status | Country | Predecessor | Successor | Remark |
---|---|---|---|---|---|---|---|---|
EN AC-43500 (DIN EN 1706 : 2020-06) | EN AC-43500 | DIN EN 1706 : 2020-06 | DIN EN 1706 : 2020-06 replaced by DIN EN 1706 : 2021-10 | Replaced | Germany | EN AC-Al Si10MnMg | EN AC-Al Si10MnMg | Aluminum casting alloy (pressure die casting). Die Legierung ist geeignet für Lebensmittelkontakt gemäß EN 601. Further properties according to EN 1706: Pressure tightness: fair Machinability (as cast): good/fair Machinability after heat treatment: good Corrosion resistance: good Weldability: good |
Chemical Composition
Cu [%] | Fe [%] | Mg [%] | Mn [%] | Si [%] | Ti [%] | Zn [%] | Source | Remark |
---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur |
Mechanical Properties
Casting Method | Condition | Tensile Strength [MPa] | Yield Strength (0.2% offset) [MPa] | Elongation A [%] | Hardness HB | HBW | Source |
---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur |
Physical Properties
Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] | Thermal Conductivity [W/(m*K)] | Electric Conductivity [MS/m] | Source |
---|---|---|---|
blur | blur | blur | blur |
Welding and Joining
Welding and Joining - Evaluation | Source |
---|---|
blur | blur |
Cross Reference
Material Name | Country | Standard | Source |
---|---|---|---|
EN AC-Al Si10MnMg | Europe | EN 1706 | |
AC4A.2 | Japan | JIS H 5202 | DIN EN 1706 : 2020-06 Annex D |
365.0 | USA | International Registration Record (AA) | DIN EN 1706 : 2020-06 Annex D |
AlSi10MnMg | |||
EN AC-AlSi10MnMg | |||
AC-43500 |
Producer/Supplier/Trade names
Tradename | Supplier |
---|---|
EN AC-Al Si10MnMg | Albert Handtmann Metallgusswerk GmbH & Co. KG, Biberach |
EN AC-Al Si10MnMg | Hydro Aluminium Deutschland GmbH , Bonn |
Silafont-36 | Rheinfelden ALLOYS GmbH & Co.KG, Rheinfelden |
Castaman-35 | Rheinfelden ALLOYS GmbH & Co.KG, Rheinfelden |
Material Compliance
REACh | RoHS |
---|---|
blur | blur |
FKM Guideline Fatigue Strength
Stress Ratio | Number of Cycles | Bending Fatigue Strength [MPa] | Source |
---|---|---|---|
blur | blur | blur | blur |
EN AC-Al Si10MnMg (EN AC-43500; DIN EN 1706 : 2020-06)
Linear-elastic
Temperature [°C] | Young's modulus [GPa] | Poisson's ratio |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
Alternating stress
Temperature [°C] | Stress ratio | Alternating stress [MPa] | Cycles |
---|---|---|---|
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Coefficient thermal expansion
Related Temperature [°C] | Temperature [°C] | Coefficient thermal expansion [10^-6*K^-1] |
---|---|---|
blur | blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Thermal conductivity
Temperature [°C] | Thermal conductivity [W/(m*K)] |
---|---|
blur | blur |
Classification
WIAM Material | Source description |
---|---|
blur | blur |
Designation
Designation | Material number | Source |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
EN AC-Al Si10MnMg (cast condition)
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Source description |
---|---|
blur | blur |
EN AC-Al Si10MnMg (T5 (cooled from an elevated temperature shaping process and then artificially aged))
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Source description |
---|---|
blur | blur |
EN AC-Al Si10MnMg (T7 (solution heat-treated and then artificially overaged))
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Source description |
---|---|
blur | blur |