CuNi2Si | CW111C Material Datasheet
Unlock Exclusive Materials Data
Gain access to a wealth of materials data by joining our Materials Portal.
Register for Free or Upgrade for Full AccessMaterial Description
Material Number | Material Number (single) | Standard | Range of Application | Standard Status | Country | Predecessor | Remark |
---|---|---|---|---|---|---|---|
CW111C (DIN EN 12163 : 2016-11) | CW111C | DIN EN 12163 : 2016-11 | Supersedes DIN EN 12163 : 2011-08 | Valid | Germany | CuNi2Si | Copper alloy rod for general purposes. |
Chemical Composition
Fe [%] | Mn [%] | Ni [%] | Pb [%] | Si [%] | Source | Remark |
---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur |
Mechanical Properties
Semi-finished Product | Strength Abbrevation | Nominal Size [mm] | Temperature [°C] | Tensile Strength [MPa] | Yield Strength (0.2% offset) [MPa] | Elongation A100 [%] | Elongation A11,3 [%] | Elongation A [%] | Hardness HB | HBW | Source |
---|---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Physical Properties
Condition | Temperature [°C] | Melting Temperature [°C] | Density [g/cm³] | Young's Modulus [GPa] | Poisson's Ratio | Mean Coefficient of Thermal Expansion [10^-6*K^-1] | Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] | Thermal Conductivity [W/(m*K)] | Mean Specific Heat Capacity [kJ/(kg*K)] | Electric Conductivity [MS/m] | Specific Electric Conductivity [% IACS] | Source | Remark |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Young's Modulus [GPa] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowMean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowHeat Treatment
Heat Treatment | Temperature [°C] | Source |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
Cross Reference
Material Name | Country | Standard | Source |
---|---|---|---|
CuNi2Si | Europe | EN 12163 | |
CuNi2Si | International | ISO 1187 | Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf |
C18000 | USA | UNS | Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf |
C64700 | USA | UNS | Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf |
B411 UNS C64700 | USA | ASTM B411 | Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf |
2.0855 | Germany | DIN 17666 | DIN CEN/TS 13388 (DIN SPEC 9700) |
CuNi2Si | Germany | DIN 17666 | DIN CEN/TS 13388 (DIN SPEC 9700) |
Producer/Supplier/Trade names
Tradename | Supplier |
---|---|
OF2400 | OTTO FUCHS KG, Meinerzhagen |
4720 | VDM Metals GmbH, Frankfurt/Main |
Coradur 2 | Wieland Prometa GmbH, Düsseldorf |
CuNi2Si | CSN Carl Schreiber GmbH, Neunkirchen |
CuNi2Si | Schreier Metall GmbH, Erkrath |
CuNi2Si | Wieland Prometa GmbH, Düsseldorf |
CuNi2Si | Auerhammer Vacuumgießerei GmbH, Aue |
Kuprodur A | VDM Metals GmbH, Frankfurt/Main |
NSB | ZOLLERN GmbH & Co. KG, Sigmaringen |
Material Compliance
REACh | RoHS |
---|---|
blur | blur |
CuNi2Si (CW111C; DIN EN 12163 : 2016-11)
Linear-elastic
Temperature [°C] | Young's modulus [GPa] | Poisson's ratio |
---|---|---|
blur | blur | blur |
blur | blur | blur |
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Coefficient thermal expansion
Related Temperature [°C] | Temperature [°C] | Coefficient thermal expansion [10^-6*K^-1] |
---|---|---|
blur | blur | blur |
Specific heat
Temperature [°C] | Specific heat [kJ/(kg*K)] |
---|---|
blur | blur |
Density
Temperature [°C] | Density [g/cm³] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Thermal conductivity
Temperature [°C] | Thermal conductivity [W/(m*K)] |
---|---|
blur | blur |
Classification
WIAM Material | Source description |
---|---|
blur | blur |
Designation
Designation | Material number | Source |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
CuNi2Si (R550; rod; 20.000-80.000mm)
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
CuNi2Si (R600; rod; 20.000-50.000mm)
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
CuNi2Si (R640; rod; 2.000-30.000mm)
Yield strength
Temperature [°C] | 0.2% Proof strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
CuNi2Si (artificially aged)
Linear-elastic
Temperature [°C] | Young's modulus [GPa] |
---|---|
blur | blur |
Thermal conductivity
Temperature [°C] | Thermal conductivity [W/(m*K)] |
---|---|
blur | blur |
Classification
Treatment | Source description |
---|---|
blur | blur |